P-878 DuraAct Power Patch Transducer

High Efficiency and Robust

  • Useable as actuator, sensor or energy generator
  • Low voltages to 120 V
  • Compact design
  • Individual solutions
P-878 DuraAct Power Patch Transducer
Product Description Specifications Downloads Quote / Order

Patch transducer

Functionality as actuator and sensor component. Nominal operating voltages of -20 to 120 V. Power generation for self-sufficient systems possible up to the milliwatt range. Can also be applied to curved surfaces.

In longitudinal direction, the DuraAct Power uses the high-efficiency d33 effect.

Robust, inexpensive design

Laminated structure consisting of PICMA® multilayer piezo element, electrodes and polymer materials. Manufactured with bubble-free injection method. The polymer coating simultaneously serves as electrical insulation and as mechanical preload, which makes the DuraAct bendable.

Customized versions and other specifications on request

  • Flexible choice of size
  • Variable design of the electrical connections
  • Combined actuator/sensor applications, even with several active piezoceramic layers
  • Arrays

Application fields

Industry and research. Can also be applied to curved surfaces or used for integration in structures. For adaptive systems, energy harvesting, structural health monitoring.

Specifications

Datasheet

Datasheet P-878

Version / Date
2020-02-12
pdf - 414 KB
Version / Date
2020-02-12
pdf - 416 KB
Version / Date
2019-02-06
pdf - 641 KB

Downloads

Datasheet

Datasheet

Datasheet P-878

Version / Date
2020-02-12
pdf - 414 KB
Version / Date
2020-02-12
pdf - 416 KB
Version / Date
2019-02-06
pdf - 641 KB

Documentation

Documentation

User Manual P876T0001

P-876, P-878 DuraAct and DuraAct Power Patch Transducers

Version / Date
2020-06-22
pdf - 617 KB
Version / Date
2020-06-22
pdf - 655 KB

Quote / Order

Ask for a free quote on quantities required, prices, and lead times or describe your desired modification. All products available online can be ordered directly.

Contact Us!

Quickly receive an answer to your question by email or phone from a local PI Ceramic sales engineer.

Compatible Electronics Related Products

Technology