Miniaturized (Shear) Cones

Customized Versions on Request

  • Shape variations, e.g. variation of the shearing angle

Specifications

Piezoceramic Mini Disks
MaterialPIC151, PIC255, PIC181
OD [mm]> 3
ID [mm]> 1
TH [mm]> 1.5
α0° < α < 90°
Electrode materialsPVD thin layer: CuNi, Au, etc.

OD    Outer diameter
ID      Inner diameter
L       Length
α       taper angle
P       Polarization direction