Rings

Outer diameter OD
To 1 mm
Inner diameter ID
To 0.2 mm
Thickness TH
To 0.15 mm (20 µm tolerance is possible)
Material
PIC151, PIC255, PIC181
Electrodes
PVD thin layer (CuNi, Au etc.)
thick layer (silver) from 0.2 mm TH

 

Variations in geometry on request

OD   Outer diameter
ID     Inner diameter
TH    Thickness
P      Polarization direction