Half and Hollow Spheres

Outer diameter OD
To 2 mm
Thickness TH

To 0.2 mm

Material
PIC151, PIC255, PIC181
Electrodes
PVD thin layer (gold), thick layer (silver)

OD  Outer diameter
TH   Thickness
P     Polarization direction