Side length (A)
2 ± 0.1 mm
Side length (B)
2 ± 0.1 mm
Thickness TH
2 ± 0.1 mm
Travel range
2.2 µm
Blocking force
>120 N
Electrical capacitance
25 nF ± 25 %
Axial resonant frequency
>600 kHz
Material
PIC252
Operating voltage range
-20 to 100 V
Operating temperature range
-40 to 150°C
Recommended preload for dynamic operation
15 MPa
Maximum preload for constant force
30 MPa
Recommended electronics
E-610, E-617, E-831