Technical Data / Ordering Numbers

Ordering NumberDisplacement [µm -10/+20%] Diameter OD [mm]Diameter ID [mm]Length L [mm ±0.5]Blocking force [N]Stiffness [N/µm]Capacitance [nF ±20%]Resonant frequency [kHz]
P-010.00H51057120023015144
P-010.05H101051214001402784
P-010.10H151051517001104067
P-010.15H20105211500765148
P-010.20H30105271800598239
P-010.30H401054016004011028
P-010.40H601055218003117021
P-016.00H51687290058042144
P-016.05H101681234003407884
P-016.10H1516815410027012067
P-016.15H2016821380019015048
P-016.20H3016827450015023039
P-016.30H4016840400010031028
P-016.40H601685247007849021
P-025.10H15251616740049022063
P-025.20H30251627870029043039
P-025.40H60251651900015092022
P-025.50H802516669600120120017

Unloaded resonant frequency measured at 1 Vpp, capacitance measured at 1 Vpp, 1 kHz. Blocking force measured at 1000 V.
Standard PZT ceramic type: PIC 151 (see page 40)
Operating voltage range: 0 to 1000 V
Operating temperature range: -20 to +85 °C
Standard mechanical interface (top & bottom): ceramic, 0.5 - 2 mm thick
Standard electrical interface: two PTFE insulated wires, pigtail length 100 mm
Available options: integrated piezo sensor or strain gauge sensors, vacuum compatible, etc.
Other specifications on request.
Specifications subject to change without notice.