Ordering NumberActive AxesDisplacement [µm -10/+20%]Cross section A x B / ID [mm]Length L [mm ±0.3]Max.Shear Load [N]Axial Stiffness [N/µm]Capacitance [nF ±20%]Resonant Frequency [kHz]
P-111.01X13 x 33.520760.5363
P-111.03X33 x 35.520451.5215
P-111.05X53 x 37.520322.5153
P-121.01X15 x 53.5502101.4363
P-121.03X35 x 55.5501304.2215
P-121.05X55 x 57.540897153
P-141.03X310 x 105.520050017215
P-141.05X510 x 107.520036028163
P-141.10X1010 x 10122002305097
P-151.03X316 x 165.5300130043215
P-151.05X516 x 167.530091071153
P-151.10X1016 x 161230058013097
P-112.01XY1 x 13 x 3520510.5 x 0.5242
P-112.03XY3 x 33 x 39.510261.5 x 1.5125
P-122.01XY1 x 15 x 55501401.4 x 1.4242
P-122.03XY3 x 35 x 59.540734.2 x 4.2125
P-122.05XY5 x 55 x 51430497 x 785
P-142.03XY3 x 310 x 109,520029017 x 17125
P-142.05XY5 x 510 x 101410020028 x 2885
P-142.10XY10 x 1010 x 10235012050 x 5051
P-152.03XY3 x 316 x 169.530074043 x 43125
P-152.05XY5 x 516 x 161430050071 x 7185
P-152.10XY10 x 1016 x 1623100310130 x 13051
P-123.01XYZ1 x 1 x 15 x 57.540891.4 x 1.4 x 2.9153
P-123.03XYZ3 x 3 x 35 x 515.510444.2 x 4.2 x 7.375
P-143.01XYZ1 x 1 x 110 x 107.52003605.6 x 5.6 x 11153
P-143.03XYZ3 x 3 x 310 x 1015.510018017 x 17 x 2975
P-143.05XYZ5 x 5 x 510 x10235012028 x 28 x 4750
P-153.03XYZ3 x 3 x 316 x 1615.530045043 x 43 x 7375
P-153.05XYZ5 x 5 x 516 x 162310030071 x 71 x 12050
P-153.10XYZ10 x 10 x 1016 x 164060170130 x 130 x 23029
P-153.10HXYZ10 x 10 x 1016 x 16 / 10402012089 x 89 x 16029
P-151.03HX316 x 16 / 105.520089030215
P-151.05HX516 x 16 / 107.520063049153
P-151.10HX1016 x 16 / 10122004008997

Unloaded resonant frequency measured at 1 Vpp, capacitance measured at 1 Vpp, 1 kHz. Standard PZT ceramic type: PIC 255 (see page 40). For more information on the shear effect see p. 34.
Operating voltage range: -250 V to +250 V
Operating temperature range: -20 to +85 °C
Standard mechanical interface (top & bottom): ceramic
Available options: integrated piezo sensor, non-magnetic, UHV, PTFE insulated wires, clear aperture etc.
Other specifications on request. Specifications subject to change without notice.