deutsch
Contact :: Impressum  

E-650 LVPZT Amplifiers for Multilayer Bender Actuators

Technical Data / Ordering Numbers

Models E-650.00 E-650.OE
Function Power amplifier Power amplifier
Channels 1 1
Maximum output power 18 W 8 W
Average output power 6 W 4 W
Peak output current 5 ms 100 mA 60 mA
Current limitation Short-circuit proof Short-circuit proof
Voltage gain 6 ± 0.1 6 ± 0.1
Polarity positive positive
Control input voltage 0 to +10 V 0 to +10 V
Display 3 digit LCD -
Output voltage 0 to 60 V,
one additional fixed voltage of 60 V
0 to 60 V,
one additional fixed voltage of 60 V
DC-offset setting 0 to 60 V at output,
with 10-turn pot (E-650.00 only)
0 to 60 V at output,
with 10-turn pot (E-650.00 only)
Input impedance 100 kW 100 kW
Frequency response 600 Hz @ 1000 nF load, 6 kHz @ no load 200 Hz @ 1000 nF load, 3 kHz no load
Control input socket BNC header pins
PZT voltage output socket 9-pin Sub-D header pins
Dimensions 160 x 125 x 50 mm 70 x 42 x 30 mm
Weight 0.7 kg (w/o P/S) 0.15 kg
Operating voltage 90-240 VAC, 50-60 Hz,
(external switching P/S, included)
+/- 15 V, 315 mA max., stabilized
Operating temperature range 0 to +50° C 0 to +50° C