PL112 - PL140 PICMATM Multilayer Bender Actuators (Bimorph)

Technical Data / Ordering Numbers

Ordering Number* Operating Voltage [V] Nominal*** displacement [µm] ±20% Free*** length [mm] Dimensions        
L x W x T [mm]
Blocking*** force [N] El. capacitance [µF] Resonant*** Frequency [Hz]
PL112.10** 0 - 60 ±80 12 17.8 x 9.6 x 0.65 ±2.0 2 x 1.1 >1000
PL122.10 0 - 60 ±250 22 25.0 x 9.6 x 0.65 ±1.1 2 x 2.4 660
PL127.10 0 - 60 ±450 27 31.0 x 9.6 x 0.65 ±1.0 2 x 3.4 380
PL128.10** 0 - 60 ±450 28 35.5 x 6.3 x 0.75 ±0.5 2 x 1.2 360
PL140.10 0 - 60 ±1000 40 45.0 x 11.0 x 0.6 ±0.5 2 x 4.0 160

* For optional 100 mm wire leads change order number extension to .x1 (e.g. PL 112.11).

*** All parameters depend on actual clamping conditions and applied load.
Operating Temperature: -20 °C to 85 (**max +150 °C
Low temperature option available
Closed-loop option on request (strain-gauge-sensor)

Other specifications on request.
Specifications subject to change without notice.