PL112 – PL140 • PD410 PICMA® Bender Piezo Actuator

All-ceramic Bender Actuators with High Displacement


  • Displacement to 2 mm
  • Fast response in the ms range
  • Nanometer resolution
  • Low operating voltage
  • Operating temperature up to 150°C
  • UHV-compatible to 10-9 hPa
  • Humidity resistance
  • Available with integrated position sensor
  • Special OEM- and bench-top amplifiers available
Displacement of the PICMA<sup>®</sup> bender actuator
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
Rectangular bender actuators
Order numberOperating voltage [V]Displacement [µm] ±20%Free length Lf [mm]Dimensions L x W x TH [mm]Blocking force [N] ±20%Electrical capacitance [µF] ±20%Resonant frequency Hz] ±20%
PL112.10*0 - 60 (±30)±801217.8 x 9.6 x 0.65±2.02 * 1.12000
PL122.100 - 60 (±30)±2502225.0 x 9.6 x 0.65±1.12 * 2.4660
PL127.100 - 60 (±30)±4502731.0 x 9.6 x 0.65±1.02 * 3.4380
PL128.10*0 - 60 (±30)±4502835.5 x 6.3 x 0.75±0.52 * 1.2360
PL140.100 - 60 (±30)±10004045.0 x 11.0 x 0.6±0.52 * 4.0160
Round bender actuators
Order numberOperating voltage [V]Displacement [µm] ±20%Free length Lf [mm]Dimensions OD x ID x TH [mm]Blocking force [N] ±20%Electrical capacitance [µF] ±20%Resonant frequency Hz] ±20%
PD410.10*0 - 60 (±30)±27044 × 7 × 0.65±202 * 10.51000
For optional 100 mm PTFE-insulated wire leads, AWG 32 (Ř 0.49 mm), change order number extension to 1 (e. g. PL112.11).
Piezo ceramic type: PIC 251, *PIC252.
Standard connections: Solderable contacts.
Resonant frequency at 1 Vpp, clamped on one side with free length Lf, without mass load. For PD410.10: Restraint with rotatable mounting on the outer circumference.
Capacitance at 1 Vpp, 1 kHz, RT.
Operating temperature range: -20 to 85°C; * -20 to 150°C.
Recommended mounting: Epoxy resin adhesive. All specifications depend on the real clamping conditions and on the applied mechanical load.
Custom designs or different specifications on request.

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.