Round bender actuators
| Order number | Operating voltage [V] | Displacement [µm] ±20% | Free length Lf [mm] | Dimensions OD x ID x TH [mm] | Blocking force [N] ±20% | Electrical capacitance [µF] ±20% | Resonant frequency Hz] ±20% |
|---|
|
| PD410.10* | 0 - 60 (±30) | ±270 | – | 44 × 7 × 0.65 | ±20 | 2 * 10.5 | 1000 |
|
| For optional 100 mm PTFE-insulated wire leads, AWG 32 (Ř 0.49 mm), change order number extension to 1 (e. g. PL112.11). |
| Piezo ceramic type: PIC 251, *PIC252. |
| Standard connections: Solderable contacts. |
| Resonant frequency at 1 Vpp, clamped on one side with free length Lf, without mass load. For PD410.10: Restraint with rotatable mounting on the outer circumference. |
| Capacitance at 1 Vpp, 1 kHz, RT. |
| Operating temperature range: -20 to 85°C; * -20 to 150°C. |
| Recommended mounting: Epoxy resin adhesive. All specifications depend on the real clamping conditions and on the applied mechanical load. |
|
| Custom designs or different specifications on request. |
|