P-010.xxH – P-025.xxH PICA Thru Ring Actuators

High-Load Piezo Actuators with Inner Hole


  • High load capacity
  • Extreme reliability: >109 cycles
  • Microsecond response
  • Sub-nanometer resolution
  • Large choice of designs
  • Large cross sections to 56 mm diameter
  • Variety of shapes
  • Vacuum-compatible and non-magnetic versions
PICA Thru are manufactured in various sizes. Standard versions are delivered with stranded wires and are covered in black. Custom designs are available on request
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
Order NumbersDisplacement [µm] (0–1000 V) -10/+20%Diameter OD [mm]Diameter ID [mm]Length L [mm] ±0.5Blocking force [N] (0–1000 V)Stiffness [N/µm]Capacitance [nF] ±20%Resonant frequency [kHz]
P-010.00H51057120023015144
P-010.10H151051517001104067
P-010.20H30105271800598239
P-010.40H601055418002918021
P-016.00H51687290058042144
P-016.10H1516815410027012067
P-016.20H3016827450015023039
P-016.40H601685247007849021
P-025.10H15251616740049022063
P-025.20H30251627870029043039
P-025.40H60251651900015092022
P-025.50H802516669600120120017
Piezo ceramic type: PIC 151.
Standard electrical interfaces: PTFE-insulated wire leads, 100 mm, AWG 24 (Ř 1.15 mm). Recommended preload for dynamic operation: 15 MPa.
Maximum preload for constant force: 30 MPa.
Resonant frequency at 1 Vpp, unloaded, free on both sides. The value is halved for unilateral clamping.
Capacitance at 1 Vpp, 1 kHz, RT.
Operating voltage: 0 to 1000 V.
Operating temperature range: -20 to 85°C.
Standard mechanical interfaces: Ceramic rings (passive PZT).
Outer surfaces: Polyolefin shrink sleeving, black (outside); epoxy resin (inside).
Custom designs or different specifications on request.

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.