P-010.xxP – P-056.xxP PICA Power Piezo Actuators

For High-Dynamics Applications


  • Operating temperature up to 150°C
  • High operating frequencies
  • High load capacity
  • Force generation up to 70 kN
  • Microsecond response
  • Sub-nanometer resolution
  • Large choice of designs
  • Large cross sections to 56 mm diameter
  • Temperature sensor PT1000 applied
  • Non-magnetic versions
PICA Power, dimensions in mm. L, OD see data table
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
Order NumberDisplacement [µm] (0–1000 V) -10/+20%Diameter OD [mm]Length L [mm] ±0.5Blocking force (0–1000 V) [N]Stiffness [N/µm]Capacitance [nF] ±20%Resonant frequency [kHz]
P-010.00P5109120024017129
P-010.10P15101818001204664
P-010.20P3010312100689037
P-010.40P60105822003718020
P-010.80P1201011123001937010
P-016.10P151618450030013064
P-016.20P301631540018025037
P-016.40P60165856009451020
P-016.80P12016111590049100010
P-016.90P1801616360003316007
P-025.10P152520990066032058
P-025.20P3025331200040063035
P-025.40P60256013000220130019
P-025.80P1202511314000120260010
P-025.90P18025165140008040007
P-035.10P15352118000120053055
P-035.20P30353423000760120034
P-035.40P60356126000430250019
P-035.80P1203511428000230520010
P-035.90P180351662900016078007
P-045.20P304536360001200210032
P-045.40P60456341000680430018
P-045.80P1204511644000370880010
P-045.90P1804516945000250130007
P-056.20P305636540001800330032
P-056.40P605663660001100670018
P-056.80P12056116680005701400010
P-056.90P1805616970000390210007
Piezo ceramic type: PIC 151.
Standard electrical interfaces: PTFE-insulated wire leads, 100 mm, AWG 24 (Ř 1.15 mm). PT1000 temperature sensor.
Recommended preload for dynamic operation: 15 MPa.
Maximum preload for constant force: 30 MPa.
Resonant frequency at 1 Vpp, unloaded. The value is halved for unilateral clamping.
Capacitance at 1 Vpp, 1 kHz, RT.
Operating voltage: 0 to 1000 V.
Operating temperature range: -20 to 150°C. Standard mechanical interfaces: Steel plates, 0.5 to 2 mm thick (depends on model).
Outer surfaces: FEP, transparent shrink sleeving (outside); epoxy resin (inside).
Custom designs or different specifications on request.

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.