| Order number | Displacement (0–1000 V) [µm] -10/+20% | Diameter OD [mm] | Length L [mm] ±0,5 | Blocking force (0–1000 V) [N] | Stiffness [N/µm] | Capacitance [nF] ±20% | Resonant frequency [kHz] |
|---|
|
| P-007.00 | 5 | 7 | 8 | 650 | 130 | 11 | 126 |
|
| P-007.10 | 15 | 7 | 17 | 850 | 59 | 33 | 59 |
|
| P-007.20 | 30 | 7 | 29 | 1000 | 35 | 64 | 36 |
|
| P-007.40 | 60 | 7 | 54 | 1150 | 19 | 130 | 20 |
|
| P-010.00 | 5 | 10 | 8 | 1400 | 270 | 21 | 126 |
|
| P-010.10 | 15 | 10 | 17 | 1800 | 120 | 64 | 59 |
|
| P-010.20 | 30 | 10 | 30 | 2100 | 71 | 130 | 35 |
|
| P-010.40 | 60 | 10 | 56 | 2200 | 38 | 260 | 20 |
|
| P-010.80 | 120 | 10 | 107 | 2400 | 20 | 510 | 10 |
|
| P-016.10 | 15 | 16 | 17 | 4600 | 320 | 180 | 59 |
|
| P-016.20 | 30 | 16 | 29 | 5500 | 190 | 340 | 36 |
|
| P-016.40 | 60 | 16 | 54 | 6000 | 100 | 680 | 20 |
|
| P-016.80 | 120 | 16 | 101 | 6500 | 54 | 1300 | 11 |
|
| P-016.90 | 180 | 16 | 150 | 6500 | 36 | 2000 | 7 |
|
| P-025.10 | 15 | 25 | 18 | 11000 | 740 | 400 | 56 |
|
| P-025.20 | 30 | 25 | 30 | 13000 | 440 | 820 | 35 |
|
| P-025.40 | 60 | 25 | 53 | 15000 | 250 | 1700 | 21 |
|
| P-025.80 | 120 | 25 | 101 | 16000 | 130 | 3400 | 11 |
|
| P-025.90 | 180 | 25 | 149 | 16000 | 89 | 5100 | 7 |
|
| P-025.150 | 250 | 25 | 204 | 16000 | 65 | 7100 | 5 |
|
| P-025.200 | 300 | 25 | 244 | 16000 | 54 | 8500 | 5 |
|
| P-035.10 | 15 | 35 | 20 | 20000 | 1300 | 700 | 51 |
|
| P-035.20 | 30 | 35 | 32 | 24000 | 810 | 1600 | 33 |
|
| P-035.40 | 60 | 35 | 57 | 28000 | 460 | 3300 | 19 |
|
| P-035.80 | 120 | 35 | 104 | 30000 | 250 | 6700 | 11 |
|
| P-035.90 | 180 | 35 | 153 | 31000 | 170 | 10000 | 7 |
|
| P-045.20 | 30 | 45 | 33 | 39000 | 1300 | 2800 | 32 |
|
| P-045.40 | 60 | 45 | 58 | 44000 | 740 | 5700 | 19 |
|
| P-045.80 | 120 | 45 | 105 | 49000 | 410 | 11000 | 10 |
|
| P-045.90 | 180 | 45 | 154 | 50000 | 280 | 17000 | 7 |
|
| P-050.20 | 30 | 50 | 33 | 48000 | 1600 | 3400 | 32 |
|
| P-050.40 | 60 | 50 | 58 | 55000 | 910 | 7000 | 19 |
|
| P-050.80 | 120 | 50 | 105 | 60000 | 500 | 14000 | 10 |
|
| P-050.90 | 180 | 50 | 154 | 61000 | 340 | 22000 | 7 |
|
| P-056.20 | 30 | 56 | 33 | 60000 | 2000 | 4300 | 32 |
|
| P-056.40 | 60 | 56 | 58 | 66000 | 1100 | 8900 | 19 |
|
| P-056.80 | 120 | 56 | 105 | 76000 | 630 | 18000 | 10 |
|
| P-056.90 | 180 | 56 | 154 | 78000 | 430 | 27000 | 7 |
|
| Piezo ceramic type: PIC 151. Standard electrical interfaces: PTFE-insulated wire leads, 100 mm, AWG 24 (Ř 1.15 mm). Recommended preload for dynamic operation: 15 MPa. |
| Maximum preload for constant force: 30 MPa. |
| Resonant frequency at 1 Vpp, unloaded, free on both sides. The value is halved for unilateral clamping. |
| Capacitance at 1 Vpp, 1 kHz, RT. |
| Operating voltage: 0 to 1000 V. |
| Operating temperature range: -20 to 85°C. |
| Standard mechanical interfaces: Steel plates, 0.5 to 2 mm thick (depends on model). |
| Outer surfaces: Polyolefin shrink sleeving, black. Custom designs or different specifications on request. |
|