P-882 – P-888 PICMA® Stack Multilayer Piezo Actuators

Ceramic-Insulated High-Power Actuators


  • Superior lifetime
  • High stiffness
  • UHV-compatible to 10-9 hPa
  • Microsecond response
  • Sub-nanometer resolution
  • Large choice of designs
  • Humidity resistance
  • Excellent temperature stability
  • Very large operating temperature range
  • Ideal for dynamic operation
PICMA<sup>®</sup> Stack actuators, L, A, B see table
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
Order number*Dimensions
A x B x L [mm]
Nominal displacement
[µm] (0 – 100 V)
Max. displacement
[µm] (0 – 120 V)
Blocking force
[N] (0 – 120 V)
Stiffness
[N/µm]
Electrical capacitance
[µF] ±20%
Resonant frequency
[kHz] ±20%
P-882.113 x 2 x 96.5 ±20%8 ±20%190240.15135
P-882.313 x 2 x 13.511 ±20%13 ±20%210160.2290
P-882.513 x 2 x 1815 ±10%18 ±10%210120.3170
P-883.113 x 3 x 96.5 ±20%8 ±20%290360.21135
P-883.313 x 3 x 13.511 ±20%13 ±20%310240.3590
P-883.513 x 3 x 1815 ±10%18 ±10%310180.4870
P-885.115 x 5 x 96.5 ±20%8 ±20%8001000.6135
P-885.315 x 5 x 13.511 ±20%13 ±20%870671.190
P-885.515 x 5 x 1815 ±10%18 ±10%900501.570
P-885.915 x 5 x 3632 ±10%38 ±10%950253.140
P-887.317 x 7 x 13.511 ±20%13 ±20%17001302.290
P-887.517 x 7 x 1815 ±10%18 ±10%17501003.170
P-887.917 x 7 x 3632 ±10%38 ±10%1850506.440
P-888.3110 x 10 x 13.511 ±20%13 ±20%35002674.390
P-888.5110 x 10 x 1815 ±10%18 ±10%36002006.070
P-888.9110 x 10 x 3632 ±10%38 ±10%380010013.040
* For optional solderable contacts, change order number extension to .x0 (e. g. P-882.10).
Piezo ceramic type: PIC 252.
Standard electrical interfaces: PTFE-insulated wire leads, 100 mm, P-882, P-883: AWG 32 (Ř 0.49 mm); P-885, P-887, P-888: AWG 30 (Ř 0.61 mm).
Recommended preload for dynamic operation: 15 MPa.
Maximum preload for constant force: 30 MPa.
Resonant frequency at 1 Vpp, unloaded, free on both sides. The value is halved for unilateral clamping.
Capacitance at 1 Vpp, 1 kHz, RT.
Operating voltage: -20 to 120 V.
Operating temperature range: -40 to 150°C.
Custom designs or different specifications on request.
Order number*Dimensions
OD x L [mm]
Nominal displacement [µm] (0 – 100 V)Max. displacement [µm] (0 – 120 V)Blocking force [N] (0 – 120 V)Stiffness [N/µm]Electrical capacitance [µF] ±20%Resonant frequency [kHz] ±20%
P-885.5511.2 x 22.514 ±10%17 ±10%850501.560
P-885.9511.2 x 40.530 ±10%36 ±10%900253.135
P-888.5518.6 x 22.514 ±10%17 ±10%34002006.060
Piezo ceramic type: PIC 252.
Standard electrical interfaces: PTFE-insulated wire leads, 100 mm, AWG 30 (Ř 0.61 mm).
Resonant frequency at 1 Vpp, unloaded, free on both sides. The value is halved for unilateral clamping. Capacitance at 1 Vpp, 1 kHz, RT.
Operating voltage: -20 to 120 V.Operating temperature range: -40 to 150°C.
Ask about custom designs!

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.