P-111 – P-151 PICA Shear Actuators

Compact Multi-Axis Actuators


  • X, XY, XZ and XYZ versions
  • Displacement to 10 µm
  • Extreme reliability: >109 cycles
  • Picometer resolution
  • Microsecond response
  • Large choice of designs
  • High resonant frequencies
  • Vacuum-compatible versions up to 10-9 hPa
  • Short leadtime
Axis and lead assignmnet for PICA Shear actuators. GND: 0 V, +: ±250 V
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
Do you have questions? Send us an e-mail!
Branch Office: *
Subject:
Last name: *
First Name: *
Title:
Company:
Department:
Street: *
Zip/Postal Code: *
City: *
Country: *
Phone:
Fax: *
E-Mail: *
Anti Spam Question*
2+2=? (enter result)
 
Message:
Please describe your application briefly:
 
Related Products:
 
PT120 – PT140 PT Piezo Tube Actuators
High-dynamics Operation with Low Loads
 

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.