P-010.xxH – P-025.xxH PICA Thru Ring Actuators

High-Load Piezo Actuators with Inner Hole


  • High load capacity
  • Extreme reliability: >109 cycles
  • Microsecond response
  • Sub-nanometer resolution
  • Large choice of designs
  • Large cross sections to 56 mm diameter
  • Variety of shapes
  • Vacuum-compatible and non-magnetic versions
PICA Thru are manufactured in various sizes. Standard versions are delivered with stranded wires and are covered in black. Custom designs are available on request
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
P-010.00H
PICA Thru Piezo Actuator, 5 µm Travel Range, 10 mm OD, 5 mm ID

P-010.10H
PICA Thru Piezo Actuator, 15 µm Travel Range, 10 mm OD, 5 mm ID

P-010.20H
PICA Thru Piezo Actuator, 30 µm Travel Range, 10 mm OD, 5 mm ID

P-010.40H
PICA Thru Piezo Actuator, 60 µm Travel Range, 10 mm OD, 5 mm ID

P-016.00H
PICA Thru Piezo Actuator, 5 µm Travel Range, 16 mm OD, 8 mm ID

P-016.10H
PICA Thru Piezo Actuator, 15 µm Travel Range, 16 mm OD, 8 mm ID

P-016.20H
PICA Thru Piezo Actuator, 30 µm Travel Range, 16 mm OD, 8 mm ID

P-016.40H
PICA Thru Piezo Actuator, 60 µm Travel Range, 16 mm OD, 8 mm ID

P-025.10H
PICA Thru Piezo Actuator, 15 µm Travel Range, 25 mm OD, 16 mm ID

P-025.20H
PICA Thru Piezo Actuator, 30 µm Travel Range, 25 mm OD, 16 mm ID

P-025.40H
PICA Thru Piezo Actuator, 60 µm Travel Range, 25 mm OD, 16 mm ID

P-025.50H
PICA Thru Piezo Actuator, 80 µm Travel Range, 25 mm OD, 16 mm ID

Custom designs or different specifications on request.

Related Products:
 
P-007 – P-056 PICA Stack Piezo Actuators
High Forces, High Displacement, Flexible Production
 
P-010.xxP – P-056.xxP PICA Power Piezo Actuators
For High-Dynamics Applications
 
PT120 – PT140 PT Piezo Tube Actuators
High-dynamics Operation with Low Loads
 

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.