PL0xx PICMA® Chip Actuators

Miniature Multilayer Piezo Actuators

PI PL0xx
    • Superior lifetime
    • Ultra-compact: From 2 mm × 2 mm × 2 mm
    • Ideal for dynamic operation
    • Microsecond response
    • Sub-nanometer resolution

Piezo Linear Actuator with PICMA® Multilayer Technology

Operating voltage -20 to 100 V. Ceramic insulation, polymer-free. Humidity resistance. UHV-compatible to 10-9 hPa, no outgassing, high bakeout temperature. Large choice of designs. Versions with rectangular or annular cross-section

Available Options

PTFE-insulated wire leads. Various geometric shapes, inner hole. Precision-ground ceramic end plates

Fields of Application

Research and industry. For laser tuning, micro-dispensing, life sciences

Specifications

Dimensions A × B × TH

Displacement

Blocking force

Capacitance

Resonant frequency

µm

N

nF

kHz

PL022.30

2 mm × 2 mm × 2 mm

2.2

>120

25

>600

PL033.30

3 mm × 3 mm × 2 mm

2.2

>300

85

>600

PL055.30

5 mm × 5 mm × 2 mm

2.2

>500

250

>600

PL088.30

10 mm × 10 mm × 2 mm

2.2

>2000

1100

>600

Travel range: at 0 to 100 V, tolerance ±20 %. The values refer to the free component and can be lower when glued on.
Blocking force: at 0 to 100 V.
Electrical capacitance: Tolerance ±20 %, measured at 1 Vpp, 1 kHz, RT.
Axial resonant frequency: measured at 1 Vpp, unloaded, unclamped. The value is halved for unilateral clamping. Lateral resonant frequencies can be lower than the axial ones, depending on the installation situation.

Piezo ceramic type: PIC252.
Standard connections: Solderable contacts. For optional PTFE-insulated wire leads, 100 mm, AWG 32, Ø 0.49 mm, change order number extension to 1 (e.g. PL022.31).
Operating voltage: -20 to 100 V.
Operating temperature range: -40 to 150 °C.
Recommended preload for dynamic operation: 15 MPa.
Maximum preload for constant force: 30 MPa.

Ask about custom designs!

Drawings / Images

PI PL0xx Drawing PI PL0xx PD0xx Inner Hole

Order Information

PICMA® Chip Actuators

PL088.30PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 10 mm × 10 mm × 2 mm

PL055.30PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 5 mm × 5 mm × 2 mm

PL033.30PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 3 mm × 3 mm × 2 mm

PL022.30PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 2 mm × 2 mm × 2 mm

 

PICMA® Chip Actuators, PTFE-insulated wire leads, 100 mm, AWG 32, Ø 0.49 mm

PL088.31PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 10 mm × 10 mm × 2 mm, Wire Leads

PL055.31PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 5 mm × 5 mm × 2 mm, Wire Leads

PL033.31PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 3 mm × 3 mm × 2 mm, Wire Leads

PL022.31PICMA® Chip Miniature Piezo Actuator, 2.2 µm Travel Range, 2 mm × 2 mm × 2 mm, Wire Leads


Ask about custom designs!

was added to the shopping cart for price quotes. OK
Click on the order information of the product you would like to add to your shopping cart for price quotes. Shopping Cart Help
To complete your quotation request, click on the shopping cart icon in the top menu bar and fill out the form. Shopping Cart Help
OK

Controllers / Drivers / Amplifiers

Related Products

Technology

Articles and Links

Downloads

fileadmin/images/filelist/pdf.png PI Datasheet PL0xx
PICMA® Chip Actuators Miniature Multilayer Piezo Actuators
PDF 837 K R1
fileadmin/images/filelist/pdf.png Kurzanleitung / Short Instructions PZ264EK
PICMA® Multilayer-Piezoaktoren / PICMA® Multilayer Piezo Actuators P-080, P-88x, PD0xx, PD410, PL0xx, PL1xx, PICMA® Stack, PICMA® Chip, PICMA® Bender
PDF 826 K 1.0.0 DE / EN
fileadmin/images/filelist/pdf.png Technical Note PL0XT0001
PL022, PL033, PL055 PICMA® Chip Monolithic Multilayer Piezo Actuators
PDF 40 K 2006-03-06 EN
fileadmin/images/filelist/pdf.png Technical Note P885T0001
Soldering PICMA® Multilayer Piezo Actuators
PDF 86 K 2006-03-06 EN