PD410 Round PICMA® Multilayer Bender Actuators

All-Ceramic Bending Actuators with High Displacement

PI PD410
    • Displacement to 500 µm
    • Fast response in the ms range
    • Nanometer resolution
    • Low operating voltage

PICMA® Multilayer Bender Elements with High Reliability

Operating voltage 0 to 60 V. Bidirectional displacement, bimorph design. Ceramic insulation, polymer-free. UHV-compatible to 10-9 hPa, no outgassing, high bakeout temperature. Reliable even under extreme conditions

Fields of Application

Research and industry, vacuum. For medical technology, laser technology, sensor systems, automation tasks, pneumatic valves

Specifications

Displacement

Dimensions

OD × ID × TH

Blocking force

Electrical capacitance

Resonant frequency

μm

N

μF

Hz

PD410.10

±240

44 mm × 7 mm × 0.65 mm

±16

2 × 10.5

1000

Displacement: Tolerance ±20 %.
Blocking force: Tolerance ±20 %.
Electrical capacitance: Tolerance ±20 %, measured at 1 Vpp, 1 kHz, RT.
Resonant frequency at 1 Vpp, restraint with rotatable mounting on the outer circumference, tolerance ±20 %.

Piezo ceramic type: PIC252.
Standard connections: Solderable contacts (PD410.10) or PTFE-insulated wire leads, 100 mm, AWG 32, Ø 0.49 mm (PD410.11).
Operating voltage: 0 to 60 (±30) V.
Operating temperature range: -20 to 150 °C.
Recommended mounting: Epoxy resin adhesive.
All parameters depend on actual clamping conditions and applied load.

Custom designs or different specifications on request.

Drawings / Images

PI PD410 Drawing

Order Information

PD410.10Circular PICMA® Multilayer Piezo Bender Actuator, ±240 µm Travel Range

With PTFE-insulated wire leads, 100 mm, AWG 32 (Ø 0.49 mm)

PD410.11Circular PICMA® Multilayer Piezo Bender Actuator, ±240 µm Travel Range, Wire Leads

Custom designs or different specifications on request.

 

 

was added to the shopping cart for price quotes. OK
Click on the order information of the product you would like to add to your shopping cart for price quotes. Shopping Cart Help
To complete your quotation request, click on the shopping cart icon in the top menu bar and fill out the form. Shopping Cart Help
OK

Controllers / Drivers / Amplifiers

Related Products

Technology

Downloads

fileadmin/images/filelist/pdf.png Technical Note PD410T0001
PD410 PICMA® Circular Bender Actuators
PDF 392 K 2014-02-10 EN
fileadmin/images/filelist/pdf.png PI Datasheet PD410
Round PICMA® Multilayer Bender Actuators All-Ceramic Bending Actuators with High Displacement
PDF 833 K
fileadmin/images/filelist/zip.png PIC Press PICMA PD410
ZIP 262 K