0399512searchresultspage3993233

P-882 – P-888 PICMA® Stack Multilayer Piezo Actuators

Ceramic-Insulated High-Power Actuators

PI P-882-P-888
    • Superior lifetime
    • High stiffness
    • Microsecond response
    • Sub-nanometer resolution
    • UHV-compatible to 10-9 hPa

Patented PICMA® Stack Multilayer Piezo Actuators with High Reliability

Operating voltage -20 to 120 V. Ceramic insulation, polymer-free. Humidity resistance. Excellent temperature stability. UHV-compatible to 10-9 hPa, no outgassing, high bakeout temperature. Ideal for dynamic operation.
Large choice of designs. Encapsulated versions for operation in splash water or oil

Custom Designs with Modified Specifications

  • For high operating temperature up to 200 °C
  • Special electrodes for currents of up to 20 A
  • Variable geometry: Inner hole, round, rectangular
  • Ceramic or metal end pieces in many versions
  • Applied SGS sensors for positional stability

Fields of Application

Science and industry. Cryogenic environment with reduced displacement. For high-speed switching, precision positioning, active and adaptive systems

Specifications

Dimensions

A × B × L

Nominal

travel range

Max.

displacement

Blocking

force

Stiffness

Electrical

capacitance

Resonant

frequency

µm

µm

N

N/µm

µF

kHz

P-882.11

3 mm × 2 mm × 9 mm

6.5

8

190

24

0.15

135

P-882.31

3 mm × 2 mm × 13.5 mm

11

13

210

16

0.22

90

P-882.51

3 mm × 2 mm × 18 mm

15*

18*

210

12

0.31

70

P-883.11

3 mm × 3 mm × 9 mm

6.5

8

290

36

0.21

135

P-883.31

3 mm × 3 mm × 13.5 mm

11

13

310

24

0.35

90

P-883.51

3 mm × 3 mm × 18 mm

15*

18*

310

18

0.48

70

P-885.11

5 mm × 5 mm × 9 mm

6.5

8

800

100

0.6

135

P-885.31

5 mm × 5 mm × 13.5 mm

11

13

870

67

1.1

90

P-885.51

5 mm × 5 mm × 18 mm

15*

18*

900

50

1.5

70

P-885.91

5 mm × 5 mm × 36 mm

32*

38*

950

25

3.1

40

P-887.31

7 mm × 7 mm × 13.5 mm

11

13

1700

130

2.2

90

P-887.51

7 mm × 7 mm × 18 mm

15*

18*

1750

100

3.1

70

P-887.91

7 mm × 7 mm × 36 mm

32*

38*

1850

50

6.4

40

P-888.31

10 mm × 10 mm × 13.5 mm

11

13

3500

267

4.3

90

P-888.51

10 mm × 10 mm × 18 mm

15*

18*

3600

200

6.0

70

P-888.91

10 mm × 10 mm × 36 mm

32*

38*

3800

100

13.0

40

Nominal travel range: at 0 to 100 V, tolerance ±20 %, * ±10 %.
Maximum travel range: at 0 to 120 V, tolerance ±20 %, * ±10 %.
Blocking force: at 0 to 120 V.
Electrical capacitance: Tolerance ±20 %, measured at 1 Vpp, 1 kHz, RT.
Resonant frequency at 1 Vpp, unloaded, unclamped. The value is halved for unilateral clamping, tolerance ±20 %.

Piezo ceramic type: PIC252.
Standard connections: PTFE-insulated wire leads, 100 mm; P-882, P-883: AWG 32 (Ø 0.49 mm); P-885, P-887, P-888: AWG 30 (Ø 0.61 mm). For optional solderable contacts, change order number extension to .x0 (e. g. P-882.10).
Operating voltage: -20 to 120 V.
Operating temperature range: -40 to 150 °C.
Recommended preload for dynamic operation: 15 MPa.
Maximum preload for constant force: 30 MPa.

Custom designs or different specifications on request.

Drawings / Images

PI P-88x PI P-882 Variety End Pieces PI P-882 - P-888 PI P-88x with Hole

Order Information

PICMA® Stack actuators, PTFE-insulated wire leads, 100 mm

P-882.11PICMA® Piezo Actuator, 6.5 µm Travel Range, 3 mm × 2 mm × 9 mm, Wire Leads

P-882.31PICMA® Piezo Actuator, 11 µm Travel Range, 3 mm × 2 mm × 13.5 mm, Wire Leads

P-882.51PICMA® Piezo Actuator, 15 µm Travel Range, 3 mm × 2 mm × 18 mm, Wire Leads

P-883.11PICMA® Piezo Actuator, 6.5 µm Travel Range, 3 mm × 3 mm × 9 mm, Wire Leads

P-883.31PICMA® Piezo Actuator, 11 µm Travel Range, 3 mm × 3 mm × 13.5 mm, Wire Leads

P-883.51PICMA® Piezo Actuator, 15 µm Travel Range, 3 mm × 3 mm × 18 mm, Wire Leads

P-885.11PICMA® Piezo Actuator, 6.5 µm Travel Range, 5 mm × 5 mm × 9 mm, Wire Leads

P-885.31PICMA® Piezo Actuator, 11 µm Travel Range, 5 mm × 5 mm × 13.5 mm, Wire Leads

P-885.51PICMA® Piezo Actuator, 15 µm Travel Range, 5 mm × 5 mm × 18 mm, Wire Leads

P-885.91PICMA® Piezo Actuator, 32 µm Travel Range, 5 mm × 5 mm × 36 mm, Wire Leads

P-887.31PICMA® Piezo Actuator, 11 µm Travel Range, 7 mm × 7 mm × 13.5 mm, Wire Leads

P-887.51PICMA® Piezo Actuator, 15 µm Travel Range, 7 mm × 7 mm × 18 mm, Wire Leads

P-887.91PICMA® Piezo Actuator, 32 µm Travel Range, 7 mm × 7 mm × 36 mm, Wire Leads

P-888.31PICMA® Piezo Actuator, 11 µm Travel Range, 10 mm × 10 mm × 13.5 mm, Wire Leads

P-888.51PICMA® Piezo Actuator, 15 µm Travel Range, 10 mm × 10 mm × 18 mm, Wire Leads

P-888.91PICMA® Piezo Actuator, 32 µm Travel Range, 10 mm × 10 mm × 36 mm, Wire Leads

 

PICMA® Stack actuators with solderable contacts

P-882.10PICMA® Piezo Actuator, 6.5 µm Travel Range, 3 mm × 2 mm × 9 mm

P-882.30PICMA® Piezo Actuator, 11 µm Travel Range, 3 mm × 2 mm × 13.5 mm

P-882.50PICMA® Piezo Actuator, 15 µm Travel Range, 3 mm × 2 mm × 18 mm

P-883.10PICMA® Piezo Actuator, 6.5 µm Travel Range, 3 mm × 3 mm × 9 mm

P-883.20PICMA® Piezo Actuator, 8.5 µm Travel Range, 3 mm × 3 mm × 11 mm

P-883.30PICMA® Piezo Actuator, 11 µm Travel Range, 3 mm × 3 mm × 13.5 mm

P-883.50PICMA® Piezo Actuator, 15 µm Travel Range, 3 mm × 3 mm × 18 mm

P-885.10PICMA® Piezo Actuator, 6.5 µm Travel Range, 5 mm × 5 mm × 9 mm

P-885.20PICMA® Piezo Actuator, 8.5 µm Travel Range, 5 mm × 5 mm × 11 mm

P-885.30PICMA® Piezo Actuator, 11 µm Travel Range, 5 mm × 5 mm × 13.5 mm

P-885.50PICMA® Piezo Actuator, 15 µm Travel Range, 5 mm × 5 mm × 18 mm

P-885.90PICMA® Piezo Actuator, 32 µm Travel Range, 5 mm × 5 mm × 36 mm

P-887.30PICMA® Piezo Actuator, 11 µm Travel Range, 7 mm × 7 mm × 13.5 mm

P-887.50PICMA® Piezo Actuator, 15 µm Travel Range, 7 mm × 7 mm × 18 mm

P-887.90PICMA® Piezo Actuator, 32 µm Travel Range, 7 mm × 7 mm × 36 mm

P-888.30PICMA® Piezo Actuator, 11 µm Travel Range, 10 mm × 10 mm × 13.5 mm

P-888.50PICMA® Piezo Actuator, 15 µm Travel Range, 10 mm × 10 mm × 18 mm

P-888.90PICMA® Piezo Actuator, 32 µm Travel Range, 10 mm × 10 mm × 36 mm


Custom designs or different specifications on request.

was added to the shopping cart for price quotes. OK
Click on the order information of the product you would like to add to your shopping cart for price quotes. Shopping Cart Help
To complete your quotation request, click on the shopping cart icon in the top menu bar and fill out the form. Shopping Cart Help
OK

Controllers / Drivers / Amplifiers

Accessories

Related Products

Technology

Articles and Links

Downloads

fileadmin/images/filelist/pdf.png Technical Note P885T0001
Soldering PICMA® Multilayer Piezo Actuators
PDF 86 K 2006-03-06 EN
fileadmin/images/filelist/pdf.png PI Datasheet P-882 – P-888
PICMA® Stack Multilayer Piezo Actuators Ceramic-Insulated High-Power Actuators
PDF 1015 K
fileadmin/images/filelist/zip.png P-88x STEP
ZIP 1 M
fileadmin/images/filelist/pdf.png Kurzanleitung / Short Instructions PZ264EK
PICMA® Multilayer-Piezoaktoren / PICMA® Multilayer Piezo Actuators P-080, P-88x, PD0xx, PD410, PL0xx, PL1xx, PICMA® Stack, PICMA® Chip, PICMA® Bender
PDF 826 K 1.0.0 DE / EN