P-840 • P-841 Preloaded Piezo Actuators

Optional with Integrated Position Sensor

PI P-840
    • Outstanding lifetime due to PICMA® piezo actuators
    • Travel range to 90 µm
    • Compact case
    • Push forces to 1000 N
    • Pull forces to 50 N
    • Microsecond response
    • Sub-nanometer resolution
    • Versions with ball tip, vacuum versions

Specifications

P-841.1
P-840.1

P-841.2
P-840.2

P-841.3
P-840.3

P-841.4
P-840.4

P-841.6
P-840.6

Unit

Tolerance

Open-loop travel, at 0 to 100 V

15

30

45

60

90

µm

±20 %

Closed-loop travel

15 / –

30 / –

45 / –

60 / –

90 / –

µm

Integrated feedback sensor*

SGS/ -

SGS/ -

SGS/ -

SGS/ -

SGS/ -

Resolution, closed-loop / open-loop**

0.3 / 0.15

0.6 / 0.3

0.9 / 0.45

1.2 / 0.6

1.8 / 0.9

nm

Static large-signal stiffness***

57

27

19

15

10

N/µm

±20 %

Push force capacity

1000

1000

1000

1000

1000

N

Pull force capacity

50

50

50

50

50

N

Torque on tip

0.35

0.35

0.35

0.35

0.35

Nm

max.

Electrical capacitance

1.5

3.0

4.5

6.0

9.0

µF

±20 %

Dynamic operating current
coefficient (DOCC)

12.5

12.5

12.5

12.5

12.5

µA/(Hz × µm)

Resonant frequency f0, no load

18

14

10

8.5

6

kHz

±20 %

Operating temperature

-20 to 80

-20 to 80

-20 to 80

-20 to 80

-20 to 80

°C

Mass without cable

20

28

46

54

62

g

±5 %

Material: case, end pieces

N-S

N-S

N-S

N-S

N-S

Length L

32

50

68

86

122

mm

±0.3

Voltage connection: LEMO FFA.00.250. Coaxial cable, RG 178, 1 m.
Sensor connector: LEMO FFA.0S.304. Coaxial cable, 1 m.
* Closed-loop models can attain linearity up to 0.15 % and are shipped with performance reports.
** The position resolution of piezo actuators is not limited by stiction or friction. Value given is noise equivalent motion with E-503 amplifier.
*** Dynamic small-signal stiffness is approx. 30 % higher.

Drawings / Images

PI P-840 Drawing PI P-841.10 Diagramm

Order Information

Actuators without sensor

P-840.10Preloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N

P-840.20Preloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N

P-840.30Preloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N

P-840.40Preloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N

P-840.60Preloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N

 

Actuators without sensor, vacuum compatible

P-840.10VPreloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, Vacuum Compatible to 10-6 hPa

P-840.20VPreloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, Vacuum Compatible to 10-6 hPa

P-840.30VPreloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, Vacuum Compatible to 10-6 hPa

P-840.40VPreloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, Vacuum Compatible to 10-6 hPa

P-840.60VPreloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, Vacuum Compatible to 10-6 hPa

 

Actuators without sensor, with tip

P-840.1BPreloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, Ball Tip

P-840.2BPreloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, Ball Tip

P-840.3BPreloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, Ball Tip

P-840.4BPreloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, Ball Tip

P-840.6BPreloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, Ball Tip

 

Actuators without sensor, with tip, vacuum compatible

P-840.1BVPreloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, Ball Tip, Vacuum Compatible to 10-6 hPa

P-840.2BVPreloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, Ball Tip, Vacuum Compatible to 10-6 hPa

P-840.3BVPreloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, Ball Tip, Vacuum Compatible to 10-6 hPa

P-840.4BVPreloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, Ball Tip, Vacuum Compatible to 10-6 hPa

P-840.6BVPreloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, Ball Tip, Vacuum Compatible to 10-6 hPa

 

Actuators with sensor

P-841.10Preloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, SGS Sensor

P-841.20Preloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, SGS Sensor

P-841.30Preloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, SGS Sensor

P-841.40Preloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, SGS Sensor

P-841.60Preloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, SGS Sensor

 

Actuators with sensor, vacuum compatible

P-841.10VPreloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, SGS Sensor, Vacuum Compatible to 10-6 hPa

P-841.20VPreloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, SGS Sensor, Vacuum Compatible to 10-6 hPa

P-841.30VPreloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, SGS Sensor, Vacuum Compatible to 10-6 hPa

P-841.40VPreloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, SGS Sensor, Vacuum Compatible to 10-6 hPa

P-841.60VPreloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, SGS Sensor, Vacuum Compatible to 10-6 hPa

 

Actuators with sensor, with tip

P-841.1BPreloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip

P-841.2BPreloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip

P-841.3BPreloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip

P-841.4BPreloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip

P-841.6BPreloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip

 

Actuators with sensor, with tip, vacuum compatible

P-841.1BVPreloaded Piezo Actuator, 15 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip, Vacuum Compatible to 10-6 hPa

P-841.2BVPreloaded Piezo Actuator, 30 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip, Vacuum Compatible to 10-6 hPa

P-841.3BVPreloaded Piezo Actuator, 45 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip, Vacuum Compatible to 10-6 hPa

P-841.4BVPreloaded Piezo Actuator, 60 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip, Vacuum Compatible to 10-6 hPa

P-841.6BVPreloaded Piezo Actuator, 90 µm Travel Range, 1000/50 N, SGS Sensor, Ball Tip, Vacuum Compatible to 10-6 hPa

was added to the shopping cart for price quotes. OK
Click on the order information of the product you would like to add to your shopping cart for price quotes. Shopping Cart Help
To complete your quotation request, click on the shopping cart icon in the top menu bar and fill out the form. Shopping Cart Help
OK

Controllers / Drivers / Amplifiers

Accessories

Technology

Articles and Links

Downloads

fileadmin/images/filelist/pdf.png Technical Note P840T0007
P-840, P-841, P-842, P-843, P-844, P-845 Preloaded Piezo Actuators
PDF 93 K 2012-03-14 EN
fileadmin/images/filelist/pdf.png PI Datasheet P-840 • P-841
Preloaded Piezo Actuators Optional with Integrated Position Sensor
PDF 781 K
fileadmin/images/filelist/zip.png P-840 P-841 STEP
ZIP 141 K