0399512searchresultspage3993233

P-007 – P-056 PICA Stack Piezo Actuators

High Forces, High Displacement, Flexible Production

PI P-007 P-056
    • Travel ranges to 300 µm
    • High load capacity
    • Force generation up to 80 kN
    • Extreme reliability: >109 cycles

Stacked piezo linear actuator

Operating voltage 0 to 1000 V. Long lifetime without derating. High specific displacement. High forces. Sub-nanometer resolution, µs response. Operating temperature range -20 to 85 °C

Available options

  • SGS sensors for positional stability
  • PZT ceramic material
  • Operating voltage range, displacement, layer thickness
  • Load capacity, force generation
  • Geometric shapes: round, rectangular
  • Mechanical interfaces: flat, spherical, metal, ceramic, glass, sapphire, etc.
  • Integrated piezoelectric detector layers
  • Special high / low temperature versions, temperature sensor
  • Vacuum-compatible and non-magnetic versions
  • Extra-tight length tolerances

Fields of application

Research and industry. For high-load positioning, precision mechanics / -machining, switches

Specifications

Displacement

Diameter OD

Length L

Blocking force

Stiffness

Electrical

capacitance

Resonant

frequency

µm

mm

mm

N

N/µm

nF

kHz

P-007.00

5

7

8

650

130

11

126

P-007.10

15

7

17

850

59

33

59

P-007.20

30

7

29

1000

35

64

36

P-007.40

60

7

54

1150

19

130

20

P-010.00

5

10

8

1400

270

21

126

P-010.10

15

10

17

1800

120

64

59

P-010.20

30

10

30

2100

71

130

35

P-010.40

60

10

56

2200

38

260

20

P-010.80

120

10

107

2400

20

510

10

P-016.10

15

16

17

4600

320

180

59

P-016.20

30

16

29

5500

190

340

36

P-016.40

60

16

54

6000

100

680

20

P-016.80

120

16

101

6500

54

1300

11

P-016.90

180

16

150

6500

36

2000

7

P-025.10

15

25

18

11000

740

400

56

P-025.20

30

25

30

13000

440

820

35

P-025.40

60

25

53

15000

250

1700

21

P-025.80

120

25

101

16000

130

3400

11

P-025.90

180

25

149

16000

89

5100

7

P-025.150

250

25

204

16000

65

7100

5

P-025.200

300

25

244

16000

54

8500

5

P-035.10

15

35

20

20000

1300

700

51

P-035.20

30

35

32

24000

810

1600

33

P-035.40

60

35

57

28000

460

3300

19

P-035.80

120

35

104

30000

250

6700

11

P-035.90

180

35

153

31000

170

10000

7

P-045.20

30

45

33

39000

1300

2800

32

P-045.40

60

45

58

44000

740

5700

19

P-045.80

120

45

105

49000

410

11000

10

P-045.90

180

45

154

50000

280

17000

7

P-050.20

30

50

33

48000

1600

3400

32

P-050.40

60

50

58

55000

910

7000

19

P-050.80

120

50

105

60000

500

14000

10

P-050.90

180

50

154

61000

340

22000

7

P-056.20

30

56

33

60000

2000

4300

32

P-056.40

60

56

58

66000

1100

8900

19

P-056.80

120

56

105

76000

630

18000

10

P-056.90

180

56

154

78000

430

27000

7

Travel range: at 0 to 1000 V, tolerance -10 / 20 %.
Length L: Tolerance ±0.5 mm.
Blocking force. at 0 to 1000 V.
Electrical capacitance: Tolerance ±20 %, measured at 1 Vpp, 1 kHz, RT.
Resonant frequency at 1 Vpp, unloaded, unclamped. The value is halved for unilateral clamping.

Piezo ceramic type: PIC151.
Standard connections: FEP-insulated wire leads, 100 mm, AWG 24, Ø 1.15 mm.
Operating voltage: 0 to 1000 V.
Operating temperature range: -20 to 85 °C.
Standard mechanical interfaces: steel plates, 0.5 to 2 mm thick (depends on model)
Outer surface: polyolefin shrink sleeving, black.
Recommended preload for dynamic operation: 15 MPa.
Maximum preload for constant force: 30 MPa.

Custom designs or different specifications on request.

Drawings / Images

PI P-007 Drawing PIC PICA Stack Customized

Order Information

P-007.00PICA Stack Piezo Actuator, 5 µm Travel Range, OD 7 mm × L 8 mm

P-007.10PICA Stack Piezo Actuator, 15 µm Travel Range, OD 7 mm × L 17 mm

P-007.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 7 mm × L 29 mm

P-007.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 7 mm × L 54 mm

P-010.00PICA Stack Piezo Actuator, 5 µm Travel Range, OD 10 mm × L 8 mm

P-010.10PICA Stack Piezo Actuator, 15 µm Travel Range, OD 10 mm × L 17 mm

P-010.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 10 mm × L 30 mm

P-010.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 10 mm × L 56 mm

P-010.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 10 mm × L 107 mm

P-016.10PICA Stack Piezo Actuator, 15 µm Travel Range, OD 16 mm × L 17 mm

P-016.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 16 mm × L 29 mm

P-016.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 16 mm × L 54 mm

P-016.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 16 mm × L 101 mm

P-016.90PICA Stack Piezo Actuator, 180 µm Travel Range, OD 16 mm × L 150 mm

P-025.10PICA Stack Piezo Actuator, 15 µm Travel Range, OD 25 mm × L 18 mm

P-025.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 25 mm × L 30 mm

P-025.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 25 mm × L 53 mm

P-025.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 25 mm × L 101 mm

P-025.90PICA Stack Piezo Actuator, 180 µm Travel Range, OD 25 mm × L 149 mm

P-025.150PICA Stack Piezo Actuator, 250 µm Travel Range, OD 25 mm × L 204 mm

P-025.200PICA Stack Piezo Actuator, 300 µm Travel Range, OD 25 mm × L 244 mm

P-035.10PICA Stack Piezo Actuator, 15 µm Travel Range, OD 35 mm × L 20 mm

P-035.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 35 mm × L 32 mm

P-035.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 35 mm × L 57 mm

P-035.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 35 mm × L 104 mm

P-035.90PICA Stack Piezo Actuator, 180 µm Travel Range, OD 35 mm × L 153 mm

P-045.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 45 mm × L 33 mm

P-045.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 45 mm × L 58 mm

P-045.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 45 mm × L 105 mm

P-045.90PICA Stack Piezo Actuator, 180 µm Travel Range, OD 45 mm × L 154 mm

P-050.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 50 mm × L 33 mm

P-050.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 50 mm × L 58 mm

P-050.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 50 mm × L 105 mm

P-050.90PICA Stack Piezo Actuator, 180 µm Travel Range, OD 50 mm × L 154 mm

P-056.20PICA Stack Piezo Actuator, 30 µm Travel Range, OD 56 mm × L 33 mm

P-056.40PICA Stack Piezo Actuator, 60 µm Travel Range, OD 56 mm × L 58 mm

P-056.80PICA Stack Piezo Actuator, 120 µm Travel Range, OD 56 mm × L 105 mm

P-056.90PICA Stack Piezo Actuator, 180 µm Travel Range, OD 56 mm × L 154 mm


Custom designs or different specifications on request.

was added to the shopping cart for price quotes. OK
Click on the order information of the product you would like to add to your shopping cart for price quotes. Shopping Cart Help
To complete your quotation request, click on the shopping cart icon in the top menu bar and fill out the form. Shopping Cart Help
OK

Controllers / Drivers / Amplifiers

Accessories

Related Products

Technology

Articles and Links

Downloads

fileadmin/images/filelist/pdf.png User Manual PZ138E
PICA Piezo Actuators: P-007, P-010, P-016, P-025, P-035, P-045, P-050, P-056 PICA Stack/Power/Thru Customized Products
PDF 922 K 1.2.0 EN
fileadmin/images/filelist/pdf.png PI Datasheet P-007 - P-056
PICA Stack Piezo Actuators High Forces, High Displacement, Flexible Production
PDF 879 K