P-010.xxP – P-056.xxP PICA Power Piezo Actuators

For High-Dynamics Applications


  • Operating temperature up to 150°C
  • High operating frequencies
  • High load capacity
  • Force generation up to 70 kN
  • Microsecond response
  • Sub-nanometer resolution
  • Large choice of designs
  • Large cross sections to 56 mm diameter
  • Temperature sensor PT1000 applied
  • Non-magnetic versions
PICA Power, dimensions in mm. L, OD see data table
 
Description   Specifications   Downloads   CAD/Video
Drawings & Images   Models   Related Info   ?? Questions ??
Bild 2 von 2

PICA Power, dimensions in mm. L, OD see data table
PICA Power, dimensions in mm. L, OD see data table

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.