Piezoceramic Patch Transducers: More Flexible for Energy Harvesting, Stuctural Health Monitoring, AdaptronicsThe patented DuraAct™ patch transducers are now even more flexible: consisting of a 0.2 mm thick piezo-ceramic film only, the P-876.SP1’s extremely compact size and robustness makes it suitable for use in very small spaces. The piezo composites become even more flexible when active films with a thickness of 80, 60 or even a mere 55 micrometers are used. Equipped with electrodes and laminated into polymer composite, these versions permit extreme bending radii of less than 10 mm. The piezo-composite element can thus also be used under the most difficult conditions. PI Ceramic has now successfully mastered the technological challenge of manufacturing and processing these extremely thin piezo ceramics.Further information: Piezo-ceramic DuraAct™ patch transducers now even thinner and more flexible back to overview |