Advanced Piezo Materials: Data, Graphed Measurements: Temperature Depencence


Temperature dependence of capacitance
C Piezoceramic Materials: PIC151, PIC255 and PIC155

Temperature dependence of resonant frequency
for the longitudinal oscillation f Piezoceramic Materials: PIC151, PIC255 and PIC155


Temperature dependence of transverse oscillation coupling factor k :
Piezoceramic Materials: PIC151, PIC255 and PIC155

Temperature dependence of the piezoelectric charge constant d :
Piezoceramic Materials: PIC151, PIC255 and PIC155


Temperature dependence of capacitance C
Piezoceramic Materials: PIC181, PIC241 and PIC300

Temperature dependence of resonant frequency for the longitudinal oscillation f
Piezoceramic Materials: PIC181, PIC241 and PIC300


Temperature dependence of transverse oscillation coupling factor k :
Piezoceramic Materials PIC181, PIC241 and PIC300

Temperature dependence of the piezoelectric charge constant d :
Piezoceramic Materials PIC181, PIC241 and PIC300


Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.