Piezoceramic actuators


Piezoceramic actuators use the effect of the relative change in length (up to approx. 1.5 0/00) when an electric field is applied. They are characterized in particular by high mechanical load capacities (up to 100 MPa), extremely low power dissipation or very low energy loss (zero current when not moving), short response times (in the submillisecond range), extremely high motion resolution (in the subnanometer range) and high reliability (more than 1010 switching cycles).
These elements are therefore destined for use in high-tech fields (semi-conductors, optics, telecommunications, etc.), and also, to an increasing extent, in the automotive field (fuel injection systems), for micropumps, pneumatic valve technology and vibration damping.
(See also the specialized catalog, “Piezo Ceramic Actuators & Custom Subassemblies”, PI Ceramic, 2003)
 



Back to overview

Assortment of multilayer actuators (PICMA series)


Assortment of piezoceramic stack actuators (high-voltage versions)

 

Headquarters


PI Ceramic GmbH
Lindenstrasse
07589 Lederhose, Germany
Phone +49 36604 882-0
E-Mail info(at)piceramic.de

Physik Instrumente (PI)
GmbH & Co. KG

Auf der Römerstrasse 1
76228 Karlsruhe/Palmbach, Germany
Phone +49 721 4846-0
E-Mail  info(at)pi.ws

Direct Offices


Distributors


Social Media









2013 PI Ceramic GmbH. All rights reserved.   ISO 9001-2008 certified.
Specifications subject to change without notice.